Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.5000 MPa | 72.52 psi | |
Dow Corning JCR 6122 Two-part, transparent, medium modulus LED encapsulant with very low viscosity, very long working time, and high transparency.Information provided by Dow Corning |