Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 7.93 MPa
1150 psi
post cured- 4 hours at 204°C
Multibase SILASTIC® C7-4565 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 7.93 MPa
1150 psi
TM R050-36
Resinlab® EP1121-4 Adhesive / Casting Resin
Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives ..
Tensile Strength, Ultimate 7.93 MPa
1150 psi
Dow Corning SILASTIC® Q7-4565 BIOMEDICAL GRADE ETR ELASTOMER
One-part, enhanced tear-resistant silicone elastomers; uncatalyzed (customer selects peroxide catalyst) elastomer materials designed for compounding into elastomer for part fabrication and medical d..
Tensile Strength, Ultimate 7.93 MPa
1150 psi
silicone property; ASTM D412
Arlon 55946C028 Silicone Rubber/Fiberglass Laminate
Side 1: cured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene
Tensile Strength, Ultimate 7.93 MPa
1150 psi
Silicone Property; ASTM D412
Arlon 920-10R##-P-1 Cured Self-Fusing Silicone Rubber Tape
1 inch wide, 20 mil thick, Red, Rectangular cross-section self-fusing silicone tape. Meets U.S. Military Specification A-A-59163 (supercedes Mil-I-46852C) except for packaging and sampling. The foll..
Tensile Strength, Ultimate 7.93 MPa
1150 psi
cured 30 days @ 25°C
Abatron AboCast 8110-2/AboCure 8110-3 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..
Tensile Strength, Ultimate 7.93 MPa
1150 psi
silicone property; ASTM D412
Arlon 56946C026 Silicone Rubber/Fiberglass Laminate
Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene
Tensile Strength, Ultimate 7.93 MPa
1150 psi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Tensile Strength, Ultimate 7.93 - 45.5 MPa
1150 - 6600 psi
Average value: 12.6 MPa Grade Count:38
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..
Copyright © lookpolymers.com All Rights Reserved