Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 7.07 MPa | 1030 psi | Cured 7 days at 25°C and 50% relative humidity |
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red RTV 159 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |
|||
Tensile Strength, Ultimate | 7.07 MPa | 1030 psi | |
Momentive Performance Materials RTV159 Red Adhesive Sealant, High Strength Paste One-part alkoxy cure. Typical uses: High-heat applications; encapsulate and seal heating elements.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance.. |