Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 68.95 MPa | 10000 psi | |
Abatron AboCast/AboCure 8109-11 All-purpose, structural dielectric resin. Better thermal and chemical properties than 8109-8, but requires heat cure. Melts at 70-80°C and remains liquid (supercooled) for many hours at RT.Process.. |
|||
Tensile Strength, Ultimate | 68.95 MPa | 10000 psi | |
Abatron AboCast/AboCure 8109-13 Liquid hardener version of AboCast/AboCure 8109-11.Processing: 100/23 pbw; Potlife: 3-5 h/20°C (68°F), 1-3 h/40°C (105°F), 0.5-1 h/60°C (140°F); mix at RT; cures in: 30 mins/60°C (140°F), 45.. |
|||
Tensile Strength, Ultimate | 68.95 MPa | 10000 psi | |
Abatron AboCast/AboCure 8109-5 High heat resistance. Easy to use.Processing: 100/20 pbw; Potlife: 7-10 days/20°C (68°F), 5-7h/60°C (140°F); mix at RT; cures in: 4 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applications.. |
|||
Tensile Strength, Ultimate | 68.95 MPa | 10000 psi | |
Abatron AboCast 50-6/AboCure 50-17 Epoxy Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Medium Amber color. Shelf life is 12+ months. |