Polymer Property : Tensile Strength, Ultimate = 68.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 68.5 MPa

@Thickness 3.17 mm
9940 psi

@Thickness 0.125 in
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Ultimate 68.5 MPa

@Thickness 3.17 mm
9940 psi

@Thickness 0.125 in
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Ultimate 68.5 MPa

@Thickness 3.17 mm
9940 psi

@Thickness 0.125 in
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).