Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 43.4 MPa
6290 psi
Indium Corp. Indalloy® 136 Bi-In-Pb-Sn Fusible Alloy
General purpose fusible alloy. Wettability not outstanding. For use as solder.Information provided by the manufacturer, Indium Corporation.
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 264E4861310 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE Butyrate 264E0096908 Natural, Trsp TENITE cellulosic plastic..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 285A2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 285A3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 550E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 565A2R30016 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 580A3720016 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
Dow AFFINITY™ SE 1400 Polyolefin Plastomer
AFFINITY® SE 1400 polyolefin plastomer is an ethylene octene resin that offers excellent performance for profile extrusion of thick tubes and good melt strength for low shear blow molding. It has e..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 465E2R30008 Natural, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 465E3720008 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 513E3720012 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..