Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
Pacific Sintered Materials FCC-214-S(HT) High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
Pacific Sintered Materials FN-262-T High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0405-45All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-T Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-45Information Provided by Pacific Sintered Metals, a division.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | |
Hogen Duralloy H10W 75 Tungsten/25 Copper PM Metal Composite RWMA Class 11.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 11 Cu-W (a hard.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | ASTM D638 |
Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Highest physical properties of GLASROD series. |
|||
Tensile Strength, Ultimate | 621 - 689 MPa | 90000 - 100000 psi | |
Materion BrushCAST® 3C High Conductivity Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | High Speed Steel (18 W, 4 Cr, 1 V) butt joint |
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin.. |
|||
Tensile Strength, Ultimate | >= 621 MPa | >= 90100 psi | Annealed; AMS 4943 |
Haynes Ti-3Al-2.5V Alloy Titanium Tubing Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | |
Mi-Tech Metals CW75 75 Tungsten/25 Copper PM Metal Composite RWMA Class 11.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 11 Cu-W (a harder mate.. |
|||
Tensile Strength, Ultimate | 621 - 896 MPa | 90000 - 130000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished Rod and Bar specifically. Other property values are typical of annealed DURANICKELÂ.. |
|||
Tensile Strength, Ultimate | >= 621 MPa | >= 90000 psi | Min per ASTM B582; Sheet and Plate |
Special Metals INCONEL® G-3 Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
Universal Wire Works 90SB-3L Steel Welding Wire The 90SB-3L alloy is the same as the 90SB-3 alloy with the exception of a restricted carbon content. Universal 90SB-3 is a 2.25% chromium and 1% molybdenum alloy for welding on steel of similar comp.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | AR-5% O2 |
Universal Wire Works ER90SB-9 Steel Welding Wire Universal 90S-B9 is used primarily for welding the higher chromium alloyed 9CrMoNbV steels A213 (T-91), A335 (p-91), A387 (Gr-91) used where elevated temperatures and pressures are required. The adv.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
Universal Wire Works 347 Stainless Steel (AMS 5680) Filler Metal Universal 347 is extensively used with the gas tungsten arc, gas metal arc and submerged arc processes. This alloy is suitable for welding stabilized steel grades 321, 347 and 348. Alloy 347 should .. |
|||
Tensile Strength, Ultimate | 621 - 758 MPa | 90000 - 110000 psi | |
Eagle Brass 7026 Copper Nickel, 1/2 Hard 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 621 - 724 MPa | 90000 - 105000 psi | |
Eagle Brass 7026 Copper Nickel, 1/4 Hard 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 621 - 758 MPa | 90000 - 110000 psi | |
Eagle Brass 70265 XP175, 1/2 Hard Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 621 - 724 MPa | 90000 - 105000 psi | |
Eagle Brass 70265 XP175, 1/4 Hard Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 621 - 724 MPa | 90000 - 105000 psi | |
Eagle Brass 725 Copper Nickel Tin, Extra Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Strength, Ultimate | 621 - 696 MPa | 90000 - 101000 psi | |
Eagle Brass 752 Nickel Silver 18%, Spring Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
Crucible Steel 303 SE Chromium-Nickel Steel Crucible 303 SE is a non-hardenable austenitic chromium-nickel steel to which selenium has been added to improve machinability and non-galling characteristics. This grade is non-magnetic in the anne.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
Crucible Steel 348 Chromium-Nickel Steel Crucible 348 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | |
CMW® ELKALOY D110 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | Annealed |
AK Steel 309S Austenitic Stainless steel AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic w.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | |
AK Steel 321 Austenitic Stainless steel AK Steel 321 is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 427 .. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | ASTM E8 |
ATI Allegheny Ludlum 309 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | |
ATI Allvac® Nickelvac® 601 UNS N06601 Nickel Superalloy Uses: Weld wire, woven wire mesh belts, rod for heat treat baskets, heat treat fixtures.Property values are for samples in the metallurgical condition: 1950°C anneal.Information provided by Allvac,.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | Annealed |
AK Steel 309 Austenitic Stainless steel AK Steel 309 provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic wh.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-214-S(HT) Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |