Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 42.7 MPa @Temperature 23.0 °C |
6190 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene AP102 Acrylonitrile Butadiene Styrene Applications:automotive componentsradiator grillsname platesknobstv componentscosmetic componentselectronic household appliances ectespecially suited for electroplating and painting articles |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6190 psi | ASTM D638 |
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate Plasticizer 8%. Weight loss on heating = 0.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6190 psi | ASTM D638 |
Buckeye Polymers BP ABS 8336 P ABS PlatingABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processing a.. |
|||
Tensile Strength, Ultimate | 42.7 MPa | 6190 psi | ASTM D638-95 |
Multibase Multi-ABS 3845 Medium Impact ABS Data provided by Multibase. |