Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 61.4 MPa | 8900 psi | ASTM D638 |
Nylene® Naxel™ PC35CV Polycarbonate Description: Naxel™ PC35CV is a 12 melt, virgin, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric .. |
|||
Tensile Strength, Ultimate | 61.4 MPa | 8900 psi | ASTM D638 |
Global PC-1418-IM Cold Temperature & Impact Modified Polycarbonate Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Ultimate | 61.4 MPa | 8900 psi | cured 8 hours @ 93°C |
Abatron AboCast 8110-9/AboCure 50-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |