Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3.94 - 321.27 MPa @Strain 0.0400 - 5.10 % |
571 - 46596 psi @Strain 0.0400 - 5.10 % |
Average value: 84.7 MPa Grade Count:6 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Tensile Strength, Ultimate | 3.94 - 321.27 MPa @Temperature -40.0 - 180 °C |
571 - 46596 psi @Temperature -40.0 - 356 °F |
Average value: 84.7 MPa Grade Count:6 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Tensile Strength, Ultimate | 3.94 - 237.87 MPa @Strain 0.0400 - 5.10 % |
571 - 34500 psi @Strain 0.0400 - 5.10 % |
Average value: 98.0 MPa Grade Count:2 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Tensile Strength, Ultimate | 3.94 - 237.87 MPa @Temperature -20.0 - 180 °C |
571 - 34500 psi @Temperature -4.00 - 356 °F |
Average value: 98.0 MPa Grade Count:2 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |