Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 134 - 324 MPa
19500 - 47000 psi
Average value: 216 MPa Grade Count:11
Overview of materials for PEKK, Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 255 - 324 MPa
37000 - 47000 psi
Eagle Brass 210 Gilding Metal, 1/4 Hard
CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi..
Tensile Strength, Ultimate 269 - 324 MPa
39000 - 47000 psi
Eagle Brass 230 Red Brass, Annealed
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Tensile Strength, Ultimate 283 - 324 MPa
41000 - 47000 psi
Eagle Brass 425 Tin Brass 2%, Annealed
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..