Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.20 MPa
464 psi
ISO 37
Multibase TPSiV® 3111-60A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Hydrolysis resistant; FDA 21 CFR 177.2600 CompliantAPPLICATIONS: Solution for soft touc..
Tensile Strength, Ultimate 3.20 MPa
464 psi
GB/T 528
Chengdu Polyster 4502 High Performance Grade TPV
Excellent resiliency, good hand feel, paintable.Information provided by Chengdu Polyster Co., Ltd.
Tensile Strength, Ultimate 3.20 MPa
464 psi
Through Plane Direction
Cymat A35620SC 040SS Stabilized Aluminum Foam
Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it ..