Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 - 46.0 MPa

@Temperature 60.0 - 120 °C
2900 - 6670 psi

@Temperature 140 - 248 °F
Average value: 33.2 MPa Grade Count:2
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
Tensile Strength, Ultimate 28.0 - 46.0 MPa

@Temperature 60.0 - 90.0 °C
4060 - 6670 psi

@Temperature 140 - 194 °F
Average value: 37.0 MPa Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe..
Tensile Strength, Ultimate 20.0 - 46.0 MPa
2900 - 6670 psi
Average value: 37.5 MPa Grade Count:16
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..