Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 31.4 MPa
4550 psi
Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy
This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atm..
Tensile Strength, Ultimate 31.4 MPa
4550 psi
ASTM D412
SK Chemicals SKYTHANE® 185A R series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 31.4 MPa
4550 psi
ASTM D412
SK Chemicals SKYTHANE® 875A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 31.4 MPa
4550 psi
ASTM D412
SK Chemicals SKYTHANE® R185A Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 31.4 MPa
4550 psi
ASTM D412
SK Chemicals SKYTHANE® T875A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 31.4 MPa
4550 psi
ASTM D412
SK Chemicals SKYTHANE® 465A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 31.4 MPa
4550 psi
ASTM D412
Lubrizol Estane® R185A Thermoplastic Polyurethane
Type: Estane® R185A is a Shore 85A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi..
Tensile Strength, Ultimate 31.4 MPa
4550 psi
after optimum cure
Armstrong A-3/A Epoxy Adhesive
A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,..
Tensile Strength, Ultimate 31.4 MPa
4550 psi
after optimum cure
Armstrong A-34 Epoxy Adhesive
This white paste material is a fast-curing adhesive with a working life of 20-25 minutes in a 100-gram mass. Mixing ratio is a convenient 1:1. A-34 has excellent wetting properties and is suggeste..