Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D638 |
Multibase Nylex™ 2185 HFX Natural Polyamide + PP Forms: PelletsProcessing Methods:Injection moldingFeatures:Tensile Strength, HighInformation provided by Multibase |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM Data |
Americas Styrenics Styron® 615APR Polystyrene
(discontinued **) STYRON® 615 APR is a general purpose easy flow resin typically used for medical, pharmaceutical and thin-walled parts. It is an excellent resin for blending with K-Resin (K-Resin is a trademark of .. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | 50 mm/min; ASTM D638 |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Tensile Strength, Ultimate | 44.1 - 80.0 MPa | 6400 - 11600 psi | Average value: 67.0 MPa Grade Count:14 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D638 |
Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D638 |
Kolon DIAMAT® IG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Tensile Strength, Ultimate | 44.1 MPa @Temperature 23.0 °C |
6400 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene KU650 Acrylonitrile Butadiene Styrene Applications:injection moldingautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances |
|||
Tensile Strength, Ultimate | 44.1 MPa @Temperature 23.0 °C |
6400 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene SP100 Acrylonitrile Butadiene Styrene Applications:injection moldinghelmetsautomotive |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | |
Indium Corp. Indalloy® 255 Bi-Pb Fusible Alloy General purpose fusible alloy. Poor solderability.Information provided by the manufacturer, Indium Corporation. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | 50 mm/min; ASTM D638 |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
SK Chemicals SKYTHANE® S368D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
SK Chemicals SKYTHANE® S392A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D638 |
SK Chemicals SKYTHANE® U101 Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
Lubrizol Estane® S160D Thermoplastic Polyurethane Type: Estane® S160D is a Shore 63D, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
Lubrizol Estane® S168D Thermoplastic Polyurethane Type: Estane® S168D is a Shore 68D, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: AsiaInformation Provided by The.. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
Lubrizol Estane® S368D Thermoplastic Polyurethane Type: Estane® S368D is a Shore 68D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
Lubrizol Estane® S385AH Thermoplastic Polyurethane Type: Estane® S385AH is a Shore 87A, polyester based thermoplastic polyurethane (TPU) with excellent transparency and Hydrolytic Stabilizer. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injectio.. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
Lubrizol Estane® S392A Thermoplastic Polyurethane Type: Estane® S392A is a Shore 93A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion, Blow .. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
Lubrizol Estane® X-590A-31 Thermoplastic Polyurethane Type: Estane® X-590A-31 is a Shore 91A, polyester grade without lubricant thermoplastic polyurethane (TPU). USP Class VI Certified.Uses: Extrusion, Film Blowing.Information Provided by The Lubrizo.. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
Lubrizol Estane® 2102-65D Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
Lubrizol Estane® 2103-55D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Load bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in .. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D638 |
Buckeye Polymers BP ABS 5425 ABS General PurposeABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of proc.. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D638 |
Buckeye Polymers BP ABS 7336 ABS High Gloss & FlowABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of pr.. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D638-95 |
Multibase Multi-ABS 3246 High Flow Grade Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
Lubrizol Estane® S375D Thermoplastic Polyurethane Type: Estane® S375D is a Shore 78D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
SK Chemicals SKYTHANE® 392A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 44.1 MPa | 6400 psi | ASTM D412 |
SK Chemicals SKYTHANE® 368D S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |