Polymer Property : Tensile Strength, Ultimate = 43500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 34.5 - 300 MPa
5000 - 43500 psi
Average value: 118 MPa Grade Count:164
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Tensile Strength, Ultimate 137 - 300 MPa
19900 - 43500 psi
Average value: 217 MPa Grade Count:30
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Tensile Strength, Ultimate 270 - 300 MPa
39200 - 43500 psi
CLAL-MSX SICLANIC S® TB Quenched Copper Alloy
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Tensile Strength, Ultimate 80.0 - 300 MPa
11600 - 43500 psi
Alliance A-5S Alnico Magnetic Material
Tensile Strength, Ultimate 80.0 - 300 MPa
11600 - 43500 psi
Alliance A-8S Alnico Magnetic Material
Tensile Strength, Ultimate 80.0 - 300 MPa
11600 - 43500 psi
Alliance A-6S Alnico Magnetic Material
Tensile Strength, Ultimate 80.0 - 300 MPa
11600 - 43500 psi
Alliance A-2S Alnico Magnetic Material
Tensile Strength, Ultimate 10.3 - 300 MPa
1500 - 43500 psi
Average value: 31.7 MPa Grade Count:167
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Tensile Strength, Ultimate 13.8 - 300 MPa
2000 - 43500 psi
Average value: 89.6 MPa Grade Count:23
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..
Tensile Strength, Ultimate 100 - 300 MPa
14500 - 43500 psi
Average value: 208 MPa Grade Count:29
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi..