Polymer Property : Tensile Strength, Ultimate = 43.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 43.4 MPa
6300 psi
ASTM D638
Technetics Group Amicon™ PVDF  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Tensile Strength, Ultimate 43.4 MPa
6290 psi
Indium Corp. Indalloy® 136 Bi-In-Pb-Sn Fusible Alloy
General purpose fusible alloy. Wettability not outstanding. For use as solder.Information provided by the manufacturer, Indium Corporation.
Tensile Strength, Ultimate 43.4 MPa
6300 psi
ASTM D638
Techmer ES Plaslube® AC-80/TF/15 Acetal (Copolymer), 15% PTFE
Plaslube polytetrafluoroethylene (PTFE) lubricated acetal copolymer grades offer additional wear and friction performance over neat acetal. Typical applications include bearings, slides and small g..
Tensile Strength, Ultimate 43.4 MPa
6300 psi
ASTM D638
American Polymers API 390 Polystyrene
API 390 is a general purpose polystyrene produced in pellet form for injection molding. API 390 has excellent clarity and easy flow.Applications: Used in the manufacture of cosmetic containers, hou..
Tensile Strength, Ultimate 43.4 MPa
6300 psi
ASTM D412/D638
Lubrizol ESTANE® 58680 Ester Based Thermoplastic Polyurethane
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 264E4861310 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE Butyrate 264E0096908 Natural, Trsp TENITE cellulosic plastic..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 285A2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 285A3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 550E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 565A2R30016 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 580A3720016 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
Dow AFFINITY™ SE 1400 Polyolefin Plastomer
AFFINITY® SE 1400 polyolefin plastomer is an ethylene octene resin that offers excellent performance for profile extrusion of thick tubes and good melt strength for low shear blow molding. It has e..
Tensile Strength, Ultimate 43.4 MPa
6300 psi
AIM 58 Fusible Alloy
Uses: lens blocking; proof casting; fusible element in safety devices; anchoring parts for machining; sealing adjustment screws; holding jet engine blades for machining and broaching; filler for sup..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 465E2R30008 Natural, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 465E3720008 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Tensile Strength, Ultimate 43.4 MPa
6290 psi
ASTM D638
Eastman Tenite Butyrate 513E3720012 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..