Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 4.48 MPa | 650 psi | |
Dow Corning HV 1760/65 Silicone Rubber 65 Shore hardness high consistency silicone rubber with fast cure system and excellent tracking and erosion resistanceInformation provided by Dow Corning |
|||
Tensile Strength, Ultimate | 4.48 MPa | 650 psi | |
Dow Corning SILASTIC® M RTV SILICONE RUBBER BASE & CLEAR CURING AGENT High durometer mold making silicone rubber suited for the reproduction of architectural, furniture components and prototypes. Silastic M is recommended for use with rigid and foam polyurethane and c.. |
|||
Tensile Strength, Ultimate | 4.48 MPa | 650 psi | |
Dow Corning SILASTIC® M RTV SILICONE RUBBER BASE & CURING AGENT (BLUE) High durometer mold making silicone rubber suited for the reproduction of architectural, furniture components and prototypes. Silastic M is recommended for use with rigid and foam polyurethane and c.. |
|||
Tensile Strength, Ultimate | 4.48 MPa | 650 psi | |
Dow Corning SILASTIC® M-2 RTV SILICONE RUBBER BASE & CURING AGENT High durometer mold making silicone rubber suited for the reproduction of architectural, furniture components and prototypes. Silastic M is recommended for use with rigid and foam polyurethane and c.. |
|||
Tensile Strength, Ultimate | 4.48 MPa | 650 psi | |
Dow Corning SILASTIC® M-3 RTV SILICONE RUBBER BASE & CURING AGENT Dow Corning Silastic® M-3 RTV Silicone Rubber is an addition cured (platinum catalyzed); high durometer silicone rubber developed for use in prototyping, architectural, and furniture applications w.. |