Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 27.0 MPa | 3910 psi | |
Shinil Chemical SHINNANO PP Polymer Nanocomposite Door Trim SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Tensile Strength, Ultimate | 27.0 MPa | 3910 psi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 250 FT EB Thermoplastic Vulcanizate Neoplast 250 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |