Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 36.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 36.5 - 44.1 MPa
5290 - 6400 psi
ASTM D638
Novatec Novacycle® 501 PVC
Novacycle® 501 is a general purpose, rigid, extrusion grade PVC compound in pellet form. This formulation is designed to provide an economical alternative for extruded profiles Raw material appe..
Tensile Strength, Ultimate 36.5 MPa
5300 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Lubri-Tech™ AS-10GB/02S Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled  (discontinued **)<
Description/Features:Glass Bead FilledSilicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 36.5 - 55.2 MPa
5300 - 8000 psi
Average value: 48.1 MPa Grade Count:7
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Thermoplastic Polyurethane Blend". Each property range of values reported is minimum and m..
Tensile Strength, Ultimate 36.5 - 241 MPa
5300 - 35000 psi
Average value: 174 MPa Grade Count:7
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..
Tensile Strength, Ultimate 36.5 - 200 MPa
5300 - 29000 psi
Average value: 147 MPa Grade Count:17
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..
Tensile Strength, Ultimate 36.5 MPa
5300 psi
ASTM D638
Techmer ES Electrafil® DB-1200/S/7/FR ABS, 7% Stainless Steel Fiber Reinforced (dry blend), Flame Retardant
Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL..
Tensile Strength, Ultimate 36.5 MPa

@Temperature 300 °C
5290 psi

@Temperature 572 °F
ASTM D638
Saint-Gobain Meldin® 7001 Direct Formed Polyimide
Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high ..
Tensile Strength, Ultimate 36.5 MPa
5300 psi
Williams Advanced Alloys WS205 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Tensile Strength, Ultimate 36.5 MPa
5300 psi
ASTM D412
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and el..
Tensile Strength, Ultimate 36.5 MPa
5300 psi
ASTM D638
American Polymers API 500 Polystyrene
API 500 is a heat resistant grade of impact polystyrene. It has superior heat resistance, good impact resistance and easy colorability.Applications: API 500 is used in housewares, toys, containers,..
Tensile Strength, Ultimate 36.5 MPa
5300 psi
ASTM D412
Lubrizol Estane® ALR PC73A Thermoplastic Polyurethane
Type: Estane® ALR PC73A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi..
Tensile Strength, Ultimate 36.5 MPa
5290 psi
ASTM D638
DuPont™ Surlyn® 9120 Ionomer Resin, Zinc
Surlyn® 9120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Tensile Strength, Ultimate 36.5 MPa
5290 psi
ASTM D638
Eastman Tenite Propionate 358A4000008 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 14%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Ultimate 36.5 MPa
5300 psi
after optimum cure
Armstrong A-1/A Epoxy Adhesive
A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El..
Tensile Strength, Ultimate 36.5 MPa
5300 psi
BCC Products BC 7062H Epoxy Casting
BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi..
Copyright © lookpolymers.com All Rights Reserved