Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.21 MPa | 321 psi | ASTM D638 |
Multibase Multi-Flex® A 0740 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowHeat StabilizedOzone ResistantProcessability, GoodSoftUV R.. |
|||
Tensile Strength, Ultimate | 2.21 MPa | 321 psi | |
Valley Adhesives EM-600 High Temperature Application Glue Stick Valley Adhesives EM-600 High Temperature Application Glue StickBonds many woods and wood composites; Excellent for woodworking and cabinetry. |