Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 31.4 - 234 MPa | 4560 - 34000 psi | Average value: 150 MPa Grade Count:15 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 31.4 MPa | 4550 psi | |
Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atm.. |
|||
Tensile Strength, Ultimate | 31.4 MPa | 4550 psi | ASTM D412 |
SK Chemicals SKYTHANE® 185A R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 31.4 MPa | 4550 psi | ASTM D412 |
SK Chemicals SKYTHANE® 875A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 31.4 MPa | 4550 psi | ASTM D412 |
SK Chemicals SKYTHANE® R185A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 31.4 MPa | 4550 psi | ASTM D412 |
SK Chemicals SKYTHANE® T875A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 31.4 MPa | 4550 psi | ASTM D412 |
SK Chemicals SKYTHANE® 465A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 31.4 MPa | 4560 psi | |
Williams Advanced Alloys WS300 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 31.4 MPa | 4550 psi | ASTM D412 |
Lubrizol Estane® R185A Thermoplastic Polyurethane Type: Estane® R185A is a Shore 85A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi.. |
|||
Tensile Strength, Ultimate | 31.4 MPa | 4550 psi | after optimum cure |
Armstrong A-3/A Epoxy Adhesive A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,.. |
|||
Tensile Strength, Ultimate | 31.4 MPa | 4550 psi | after optimum cure |
Armstrong A-34 Epoxy Adhesive This white paste material is a fast-curing adhesive with a working life of 20-25 minutes in a 100-gram mass. Mixing ratio is a convenient 1:1. A-34 has excellent wetting properties and is suggeste.. |