Polymer Property : Tensile Strength, Ultimate = 3.94 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.94 - 321.27 MPa

@Strain 0.0400 - 5.10 %
571 - 46596 psi

@Strain 0.0400 - 5.10 %
Average value: 84.7 MPa Grade Count:6
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Tensile Strength, Ultimate 3.94 - 321.27 MPa

@Temperature -40.0 - 180 °C
571 - 46596 psi

@Temperature -40.0 - 356 °F
Average value: 84.7 MPa Grade Count:6
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Tensile Strength, Ultimate 3.94 - 237.87 MPa

@Strain 0.0400 - 5.10 %
571 - 34500 psi

@Strain 0.0400 - 5.10 %
Average value: 98.0 MPa Grade Count:2
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
Tensile Strength, Ultimate 3.94 - 237.87 MPa

@Temperature -20.0 - 180 °C
571 - 34500 psi

@Temperature -4.00 - 356 °F
Average value: 98.0 MPa Grade Count:2
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..