Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 188 MPa | 27300 psi | 5mm/min; ISO 527 |
BASF Ultramid® B3WG7 BK00564 35% Glass Filled PA6 (Dry) Ultramid B3WG7 BK00564 is a 35% glass fiber reinforced, pigmented black, injection molding PA6 grade for highly rigid, dimensionally stable components which are resistant to high
temperature aging a.. |
|||
Tensile Strength, Ultimate | 188 MPa | 27300 psi | 5mm/min; ASTM D638 |
Asia International Enterprise (Hong Kong) 60G6-33GF Nylon 66, 33% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |