Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 260 MPa | 37700 psi | ISO 527 |
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Tensile Strength, Ultimate | 260 MPa | 37700 psi | dry; ISO 527-1/-2 |
DSM Stanyl® TW271B6 (PA46+PTFE)-CF30 30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Tensile Strength, Ultimate | 260 MPa | 37700 psi | |
Ametek Ultra 316L P/M Stainless Steel, Sintered from 6.22 g/cc Green Density Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement i.. |
|||
Tensile Strength, Ultimate | 260 - 350 MPa | 37700 - 50800 psi | |
ArcelorMittal 54+AS Aluminized steel Use: Difficult drawingInformation provided by ArcelorMittal |
|||
Tensile Strength, Ultimate | 260 - 350 MPa | 37700 - 50800 psi | |
ArcelorMittal 56+AS Aluminized steel Use: Extra-deep drawingInformation provided by ArcelorMittal |
|||
Tensile Strength, Ultimate | 260 - 350 MPa | 37700 - 50800 psi | |
ArcelorMittal 57+AS Aluminized steel Use: Extra-deep drawingInformation provided by ArcelorMittal |
|||
Tensile Strength, Ultimate | 260 MPa | 37700 psi | ASTM D638 |
Owens Corning Glass Fiber Reinforced Polyester, Woven Roving (Lay-up), 50 wt.% glass Data provided by the manufacturer, Owens Corning. |