Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | TM R050-36 |
Resinlab® EP1294 Mineral Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1294 is a two part mineral filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-exti.. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | ASTM D412 |
PB1100-60 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | |
Sylvin Technologies 6160-90 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | |
Sylvin Technologies 6161-82 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | |
Sylvin Technologies 8925-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | |
Sylvin Technologies 8960-90 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | |
Sylvin Technologies 916V0-95 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | |
Sylvin Technologies 9925-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | |
Sylvin Technologies 500 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | |
Sylvin Technologies 5132-75 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | |
Sylvin Technologies 578 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | |
Sylvin Technologies 6065 LT GL 85 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | |
Sylvin Technologies 6137-85 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | ASTM D638 |
Ecomass® 4703ZD90 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polym.. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | ASTM D638 |
Ecomass® 705ZG91 Stainless Steel/Tungsten Filled ABS High Specific GravityStainless Steel/Tungsten Powder Filled ABSInformation provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | ASTM D638 |
Ecomass® 720ZD91 Tungsten Filled ABS High Specific GravityTungsten Powder Filled ABSGood ToughnessPlateableInformation provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | ASTM D638 |
Colorite Polymers 7588 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
Tensile Strength, Ultimate | 16.5 MPa | 2400 psi | |
Sylvin Technologies 5123 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 16.55 MPa | 2400 psi | 500 mm/min; ASTM D412 |
DuPont Performance Polymers Kalrez® 6230 FFKM Perfluoroelastomer Kalrez® parts made from compounds 6230 provide superior chemical resistance and low contamination from extractables in pharmaceutical and food handling applications where FDA compliance is required.. |