Polymer Property : Tensile Strength, Ultimate = 24.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 24.8 MPa
3600 psi
ASTM D638
Chevron Phillips HiD® 9075 HDPE Injection Molding Resin  (discontinued **)
Resin Type: linear copolymer; ASTM D3350 Classification 335540A; ASTM D4976 Classification: PE 235, A 54607Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, e..
Tensile Strength, Ultimate 24.8 MPa
3600 psi
Sylvin Technologies 9604-90C Clear PVC for Injection Molding
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 24.8 MPa
3600 psi
ASTM D638
DuPont™ Surlyn® 9910 Ionomer Resin, Zinc
Surlyn® 9910 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Tensile Strength, Ultimate 24.8 MPa
3600 psi
Molded property
Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade
DOWLEX® 2049 Polyethylene resin offers excellent tear strength, medium stiffness, outstanding toughness and puncture resistance for films used in food contact applications. When used unmodified and..
Tensile Strength, Ultimate 24.8 MPa
3600 psi
508 mm/min; ASTM D638
Dow Engage® 8450 Polyolefin Elastomer
Description: Engage® 8450 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p..
Tensile Strength, Ultimate 24.8 MPa
3600 psi
ASTM D412
Colorite Polymers CS1533UL Wire and Cable Jacket Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
Tensile Strength, Ultimate 24.8 MPa
3600 psi
ASTM D412
Colorite Polymers CS1534SR Wire and Cable Insulation Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
Tensile Strength, Ultimate 24.8 MPa
3600 psi
ASTM D638
Colorite Polymers 92-1107 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 24.8 MPa
3600 psi
2 in/min (50 mm/min); ASTM D638
Bapolene® 4012 Polypropylene, Extrusion Grade
Bapolene PP4012 is a general purpose extrusion resin with excellent stiffness and processability, chemical resistance, and ESCR properties. This product meets FDA standards for food contact applic..
Tensile Strength, Ultimate 24.8 MPa
3600 psi
ASTM D412/D638
Lubrizol ESTANE® 58224 Ester Based Thermoplastic Polyurethane
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 24.8 MPa
3600 psi
ASTM D638
Buckeye Polymers BP RPP 1010 TR Blk Reprocessed Polypropylene, 10% Mineral Filled
Talc Filled BlackThis reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin comp..