Polymer Property : Tensile Strength, Ultimate = 220 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 220 MPa
31900 psi
Osprey Metals CE17M Al-Si Controlled Expansion Alloy
Al-27%Si+ controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
Tensile Strength, Ultimate 220 MPa
31900 psi
MarkeTech Aluminum Oxide Ceramic - Alumina 99.5%
Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture..
Tensile Strength, Ultimate 220 MPa
31900 psi
GBC Grade 99 Alumina
Data provided by the manufacturer, GBC Materials Corporation.
Tensile Strength, Ultimate 220 MPa

@Temperature 980 °C
31900 psi

@Temperature 1800 °F
Haynes Waspaloyâ„¢ alloy, sheet
Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go..
Tensile Strength, Ultimate 220 MPa
31900 psi
dry; ISO 527-1/-2
DSM Novamid® 1013G45 1 NA PA6-GF45
45% Glass Reinforced, Injection Molding
Tensile Strength, Ultimate 220 MPa
31900 psi
dry; ISO 527-1/-2
DSM Novamid® 1013GH45 1 NA/BK701 PA6-GF45
45% Glass Reinforced, Heat Stabilized, Injection Molding
Tensile Strength, Ultimate 220 MPa
31900 psi
dry; ISO 527-1/-2
DSM EcoPaXX® Q-HG10 PA410-GF50
50% Glass Reinforced, Heat Stabilized
Tensile Strength, Ultimate 220 MPa
31900 psi
Worked
CMW® D505F Silver Nickel Contact Material
For electrical contacts.Information provided by CMW Inc.