Polymer Property : Tensile Strength, Ultimate = 21500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 148 MPa
21500 psi
ASTM D638
Chem Polymer Chemlon 225 G Nylon 6, 25% Glass Fiber Reinforced
A 25% glass fiber reinforced nylon 6 offering a balance of properties between the 20% (Chemlon 220 G) and 30% (Chemlon 233 G) product offerings. This product offers further improvements in tensile ..
Tensile Strength, Ultimate 148 MPa
21500 psi
ASTM D638
A. Schulman ComAlloy Voloy® 682 Nylon 6/6, Glass Fiber, Nylon 6/6 Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman product line.