Polymer Property : Tensile Strength, Ultimate = 211 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 26.6 - 211 MPa
3860 - 30600 psi
Average value: 144 MPa Grade Count:52
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Tensile Strength, Ultimate 54.0 - 211 MPa

@Temperature -40.0 - 150 °C
7830 - 30600 psi

@Temperature -40.0 - 302 °F
Average value: 78.5 MPa Grade Count:5
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..