Polymer Property : Tensile Strength, Ultimate = 21.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 21.4 - 30.3 MPa
3100 - 4390 psi
Average value: 26.2 MPa Grade Count:5
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is ..
Tensile Strength, Ultimate 21.4 MPa
3100 psi
ASTM D638
American Polymers API 650-21 Polystyrene
API 650-21 has been developed for injection molding applications that need a higher degree of toughness and gloss than conventional polystyrene. This polymer approaches ABS type properties.Applicat..
Tensile Strength, Ultimate 21.4 MPa
3100 psi
ASTM D638
Ecomass® 4703ZD84 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technica..
Tensile Strength, Ultimate 21.4 MPa
3100 psi
ASTM D638
Colorite Polymers 9833 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 21.4 MPa
3100 psi
ASTM D412
Colorite Polymers Weatherflex™ CS1534WX (NTL02P) Wire and Cable Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
Tensile Strength, Ultimate 21.4 MPa
3100 psi
ASTM D412
Dow SPECTRIM™ 50-S Reaction Moldable Polymer
SPECTRIM™ 50-S reaction moldable polymer is a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology developed by the Dow Chemical Company.Information p..
Tensile Strength, Ultimate 21.4 MPa
3100 psi
ASTM D638
Colorite Polymers 9588 Non-Phthalate 88 Series Vinyl Compound
Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo..
Tensile Strength, Ultimate 21.4 MPa
3100 psi
ASTM D412
Colorite Polymers CS1534SR Wire and Cable Insulation Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
Tensile Strength, Ultimate 21.4 - 32.0 MPa
3100 - 4640 psi
Average value: 27.8 MPa Grade Count:3
Overview of materials for Linear Low Density Polyethylene (LLDPE), Sheeting Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Sheeting Grade". Each property range of values reported is mini..
Tensile Strength, Ultimate 21.4 MPa
3100 psi
ASTM D638
Adell RZ-16 Copolymer Polypropylene, 30% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.