Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 1800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 12.41 MPa
1800 psi
Pyrotek Pyroboard™ S400 Roller
Pyroboard™ S400 is a low temperature material that is normally used in cooling zones where water quenching is present.Information provided by Pyrotek.
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM D638
NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin
Features: Excellent tensile properties, excellent impact toughness, outstanding gloss and clarity, excellent processability.Applications: Coating and sheathing.Data provided by the manufacturer.
Tensile Strength, Ultimate 12.4 MPa
1800 psi
TM R050-36
Resinlab® EP1340 Medium Viscosity, Flame Retardant Epoxy Casting Resin System
Resinlab™ EP1340 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034) for U..
Tensile Strength, Ultimate 12.4 - 76.0 MPa
1800 - 11000 psi
Average value: 26.9 MPa Grade Count:206
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM D638
Multibase Multi-Flex® A 9402 MR TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
Sylvin Technologies 8960-75 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 12.4 MPa
1800 psi
Sylvin Technologies 9960-75 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 12.4 MPa
1800 psi
Sylvin Technologies 9980-95 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM-D1457
CoorsTek PolyGlyde™ 5400 Self-Lubricating Seal
PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
Molded property
Dow LDPE 681I Low Density Polyethylene, Liner Film Grade
DOW LDPE 681I resin is a barefoot general purpose medium duty liner film resin for packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact appl..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM D-638
CMT Materials REN Shape® 460 Prototype Tool & Precision Modeling Board
REN Shape 460 is a moderate density precision modeling board that features a lower coefficient of thermal expansion to provide enhanced dimensional stability over a broader temperature range than ot..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM D412
Colorite Polymers Weatherflex™ CS1522WX (NTL01B) Wire and Cable Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
Dow HDPE 10462N High Density Polyethylene
DOW HDPE 10462N resin is a narrow molecular weight distribution polymer designed to offer good stress crack resistance and impact strength with excellent rigidity. This resin has good processability..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM D638
Colorite Polymers 6500 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM D638
Colorite Polymers 6507 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM D638
Colorite Polymers 8818 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 1070 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
Cured property; ASTM D412
Aptek 2506-A/B Room temperature curing, low modulus urethane conformal coating
Room temperature curing, low modulus urethane conformal coatingAPTEK 2506-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the e..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b..
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM D638
Buckeye Polymers BP Flex D4507 TPO
TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a..
Tensile Strength, Ultimate 12.4 - 48.3 MPa
1800 - 7000 psi
Average value: 26.2 MPa Grade Count:55
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..
Copyright © lookpolymers.com All Rights Reserved