Polymer Property : Tensile Strength, Ultimate = 18.44 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 18.44 MPa
2675 psi
Type 4 - Flexibles, 20 in/min; ASTM D638
PolyOne Geon® XV3811B Thermoplastic Elastomer - PVC/TPU  (discontinued **)
Applications:Hose and TubingCustom ProfilesProcessing Method:Extrusion and MoldingExtrusion-ProfileInformation provided by PolyOne Corporation.