Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 16.6 MPa | 2410 psi | 20" / min.; ASTM D-683-95 |
Multibase Multi-Flex® TPO D-5016 Multi-Flex® D-5016 is an elastomer modified polypropylene for applications requiring elastomeric properties and good molding behavior.Data provided by Multibase. |