Polymer Property : Tensile Strength, Ultimate = 1570 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.8 MPa
1570 psi
Across Flow; ASTM D412
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Tensile Strength, Ultimate 10.8 MPa
1570 psi
Across Flow; ASTM D412
ExxonMobil Vyram™ 9203-45 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
Tensile Strength, Ultimate 10.8 MPa
1570 psi
ISO 37
Kuraray SEPTON® S2063 Thermoplastic Rubber
SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi..
Tensile Strength, Ultimate 10.8 MPa
1570 psi
Kuraray SEPTON® S64 Soft Compound
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its unique isoprene technology. SEPTON® resins are a series of hydrogenated styre..
Tensile Strength, Ultimate 10.8 MPa
1570 psi
Dow LDPE 640IM Low Density Polyethylene
DOW LDPE 640IM resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate stiffness for general purpose, and cap..
Tensile Strength, Ultimate 10.8 MPa
1570 psi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 2090 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Tensile Strength, Ultimate 10.8 MPa
1570 psi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 4680 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Tensile Strength, Ultimate 10.8 MPa
1570 psi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 2090 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Copyright © lookpolymers.com All Rights Reserved