Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1520 MPa
220000 psi
50% Cold Rolled
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers..
Tensile Strength, Ultimate 1520 MPa
220000 psi
700°F Temper Temperature
Latrobe Lescalloy® 4335+V VAC-ARC High Strength Alloy Steel
4335+V VAC-ARC is a low alloy steel with good strength and high hardenability. In addition, uniform properties are obtained in large sections. The alloy can be heat treated to strength values with..
Tensile Strength, Ultimate 1520 MPa
220000 psi
24°C Test Temp
Latrobe CBS-600â„¢ VIM-VAR Carburizing Bearing and Gear Steel
CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. Double vacuum melting is employed to provide optimum tensile properties as well as describe..
Tensile Strength, Ultimate >= 1520 MPa
>= 220000 psi
H950 Condition - 500°C
Latrobe Lescalloy® 13-8 Mo VIM-VAR Precipitation Hardening Stainless Steel
Lescalloy 13-8 Mo VIM-VAR is a precipitation hardening martensitic stainless steel offering excellent fracture toughness and transverse mechanical properties coupled with the resistance to stress-co..
Tensile Strength, Ultimate 1520 MPa
220000 psi
Specialty Materials 5521 Boron Epoxy Prepreg Tape
Specialty Materials' 5521 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, epoxy resin. Performing at temperatures up to 350°F,..
Tensile Strength, Ultimate 1520 MPa
220000 psi
Aged to ~ 46 HRC
Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel
A precipitation hardening stainless steel which offers excellent high corrosion resistance, excellent dimensional stability during hardening and good wear resistance. It can be used at its as-suppli..
Tensile Strength, Ultimate 1520 MPa
220000 psi
Latrobe Lescalloy® HY-TUF VAC-ARC High Strength Alloy Steel
LESCALLOY HY-TUF VAC-ARC steel is a high strength low alloy steel. It is typically used in the 220/240 ksi (1517/1655 MPa) tensile strength range. At this strength level, the alloy has good ductilit..
Tensile Strength, Ultimate 1520 MPa
220000 psi
Oil Quenched from 871°C; 538°C Temper Temperature
Latrobe Staminal™ Shock Resisting Die Steel
Staminal is an air or oil hardening die steel containing a large percentage of nickel combined with a proper balance of other alloying elements for deep hardening and extreme toughness. For tools, ..