Polymer Property : Tensile Strength, Ultimate = 1470 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.1 MPa
1470 psi
no post cure, press cured for 5 minutes; ASTM D412
Multibase SILASTIC® Q7-4850 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tensile Strength, Ultimate 10.1 MPa
1470 psi
Dow Corning SILASTIC® LS-2840 FLUOROSILICONE RUBBER
40 Durometer, off-white, uncatalysed, moulding grade fluorosilicone baseInformation provided by Dow Corning
Tensile Strength, Ultimate 10.1 MPa
1470 psi
Dow Corning SILASTIC® Q7-4850 BIOMEDICAL GRADE ETR ELASTOMER, KIT
Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning