Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.0 - 100 MPa
8990 - 14500 psi
Average value: 93.8 MPa Grade Count:7
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Tensile Strength, Ultimate 15.0 - 100 MPa
2180 - 14500 psi
Average value: 71.3 MPa Grade Count:141
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Tensile Strength, Ultimate 80.0 - 100 MPa
11600 - 14500 psi
ASTM D638
Chang Chun Plastic PBT3015 15% Glass Fiber Enforced PBT
Information provided by Dowell Trading Company Ltd.
Tensile Strength, Ultimate 40.0 - 100 MPa

@Temperature -40.0 - 80.0 °C
5800 - 14500 psi

@Temperature -40.0 - 176 °F
Average value: 71.0 MPa Grade Count:1
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
Tensile Strength, Ultimate 82.7 - 100 MPa
12000 - 14500 psi
Average value: 91.9 MPa Grade Count:7
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu..
Tensile Strength, Ultimate 35.0 - 100 MPa

@Temperature -40.0 - 70.0 °C
5080 - 14500 psi

@Temperature -40.0 - 158 °F
Average value: 67.5 MPa Grade Count:4
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Tensile Strength, Ultimate 33.0 - 100 MPa
4790 - 14500 psi
Average value: 47.4 MPa Grade Count:29
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
Tensile Strength, Ultimate 10.0 - 100 MPa

@Temperature -20.0 - 100 °C
1450 - 14500 psi

@Temperature -4.00 - 212 °F
Average value: 45.0 MPa Grade Count:2
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
Tensile Strength, Ultimate 10.0 - 100 MPa

@Strain 1.00 - 8.00 %
1450 - 14500 psi

@Strain 1.00 - 8.00 %
Average value: 45.0 MPa Grade Count:2
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
Tensile Strength, Ultimate 70.0 - 100 MPa

@Temperature -40.0 - -40.0 °C
10200 - 14500 psi

@Temperature -40.0 - -40.0 °F
Average value: 85.0 MPa Grade Count:4
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..