Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 98.1 MPa
14200 psi
DIN 53455; ASTM D638
Kolon KOPET® KP133135 FR-PET Resin  (discontinued **)
KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of p..
Tensile Strength, Ultimate 98.0 MPa
14200 psi
ISO 527
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Tensile Strength, Ultimate 98.0 MPa
14200 psi
ISO 527
LATI LARIL 13 G/20-V1 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Tensile Strength, Ultimate 97.9 MPa
14200 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® SF-20GF/000 Polyphenylene Sulfide (PPS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 98.1 MPa
14200 psi
DIN 53455; ASTM D638
Kolon KOPA® KN333G15HI Multi Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Tensile Strength, Ultimate 97.9 MPa

@Thickness 3.17 mm
14200 psi

@Thickness 0.125 in
ASTM D638
LG Chemical Lupox® PBT-GP-2156F 15% GFR Flame Retardant PBT
General Purpose PBT, 15% Glass Fiber Reinforced, Weather Resistant, Flame Retardant, Non-Bleed. Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Ultimate 98.1 MPa
14200 psi
Shinil Chemical SHINCON PPS Electro Conductive Polymer
SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's ..
Tensile Strength, Ultimate 98.1 MPa
14200 psi
Shinil Chemical SHINCON PPS-CNT LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..
Tensile Strength, Ultimate 98.0 MPa
14200 psi
ASTM D638
Tipco Tipcolene® SEB 300 - 30% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability
30% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Tensile Strength, Ultimate 98.0 MPa
14200 psi
ATSM D638
Ashley Polymers Ashlene® 126 PBT Polyester, 30% Glass Reinforced
General purpose 30% glass reinforcement, natural. Colors will modify properties.Data provided by the manufacturer
Tensile Strength, Ultimate 98.1 MPa
14200 psi
5mm/min; ASTM D638
Asia International Enterprise (Hong Kong) 30G3F Polybutylene terephthalate, 15% Glass Fiber Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Tensile Strength, Ultimate 98.0 MPa
14200 psi
ATSM D638
Ashley Polymers Ashlene® 126WO PBT Polyester, 30% Glass Reinforced
PBT polyester with 30% glass reinforcement, flame retardant, natural. Colors will modify properties.Data provided by the manufacturer
Tensile Strength, Ultimate 98.0 MPa
14200 psi
5mm/min; ISO 527
BASF Ultradur S 4090 G4 BK5110 20% Glass Filled PBT
Ultradur S 4090 G4 BK5110 is a 20% glass reinforced, pigmented black PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkag..
Tensile Strength, Ultimate 98.1 MPa
14200 psi
5mm/min; ASTM D638
Asia International Enterprise (Hong Kong) 30G3 Polybutylene terephthalate, 15% Glass Fiber Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.