Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 9.80 - 11.7 MPa | 1420 - 1700 psi | Average value: 10.9 MPa Grade Count:4 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade". Each property range of values reported is min.. |
|||
Tensile Strength, Ultimate | 9.80 MPa | 1420 psi | ASTM D638 |
ExxonMobil Escorene® MV-02528 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Tensile Strength, Ultimate | 9.81 - 52.0 MPa | 1420 - 7540 psi | Average value: 24.6 MPa Grade Count:28 |
Overview of materials for PVC, Sheet Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Ultimate | 9.81 MPa | 1420 psi | ASTM D638 |
SK Chemicals SKYTHANE® US106B Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 9.79 MPa | 1420 psi | |
Dow Corning SILASTIC® 9280/30 KIT PARTS A&B 40 Durometer, 2-part, 1 to 1 mix, translucent Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Tensile Strength, Ultimate | 9.80 MPa | 1420 psi | |
Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2553 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and impact strength with excellent stiffness for hou.. |
|||
Tensile Strength, Ultimate | 9.80 MPa | 1420 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8452 Polyolefin Elastomer Description: Engage® 8452 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent toughness, softness, and optical properties. It has excellent compatibility with other polyolefin.. |
|||
Tensile Strength, Ultimate | 9.80 - 37.3 MPa | 1420 - 5410 psi | Average value: 23.1 MPa Grade Count:25 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |