Polymer Property : Tensile Strength, Ultimate = 13.79 MPa
Polymer Property :
Tensile Strength, Ultimate =
13.79 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
13.79
MPa
2000
psi
Multibase Multi-Flex® D 5308 HF Black TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsInformation provided by Multibase