Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 30.0 - 128 MPa | 4350 - 18500 psi | Average value: 68.4 MPa Grade Count:58 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Tensile Strength, Ultimate | 31.0 - 128 MPa | 4500 - 18500 psi | Average value: 79.1 MPa Grade Count:17 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Tensile Strength, Ultimate | 5.00 - 128 MPa | 725 - 18500 psi | Average value: 28.2 MPa Grade Count:238 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |