Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | ASTM D638 |
NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin Features: Excellent tensile properties, excellent impact toughness, outstanding gloss and clarity, excellent processability.Applications: Coating and sheathing.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | TM R050-36 |
Resinlab® EP1340 Medium Viscosity, Flame Retardant Epoxy Casting Resin System Resinlab™ EP1340 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034) for U.. |
|||
Tensile Strength, Ultimate | 12.4 - 76.0 MPa | 1800 - 11000 psi | Average value: 26.9 MPa Grade Count:206 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | ASTM D638 |
Multibase Multi-Flex® A 9402 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | |
Sylvin Technologies 8960-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | |
Sylvin Technologies 9960-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | |
Sylvin Technologies 9980-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | ASTM-D1457 |
CoorsTek PolyGlyde™ 5400 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | Molded property |
Dow LDPE 681I Low Density Polyethylene, Liner Film Grade DOW LDPE 681I resin is a barefoot general purpose medium duty liner film resin for packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact appl.. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | ASTM D-638 |
CMT Materials REN Shape® 460 Prototype Tool & Precision Modeling Board REN Shape 460 is a moderate density precision modeling board that features a lower coefficient of thermal expansion to provide enhanced dimensional stability over a broader temperature range than ot.. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | ASTM D412 |
Colorite Polymers Weatherflex™ CS1522WX (NTL01B) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | |
Dow HDPE 10462N High Density Polyethylene DOW HDPE 10462N resin is a narrow molecular weight distribution polymer designed to offer good stress crack resistance and impact strength with excellent rigidity. This resin has good processability.. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | ASTM D638 |
Colorite Polymers 6500 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | ASTM D638 |
Colorite Polymers 6507 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | ASTM D638 |
Colorite Polymers 8818 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 1070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | Cured property; ASTM D412 |
Aptek 2506-A/B Room temperature curing, low modulus urethane conformal coating Room temperature curing, low modulus urethane conformal coatingAPTEK 2506-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the e.. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Tensile Strength, Ultimate | 12.4 MPa | 1800 psi | ASTM D638 |
Buckeye Polymers BP Flex D4507 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Tensile Strength, Ultimate | 12.4 - 48.3 MPa | 1800 - 7000 psi | Average value: 26.2 MPa Grade Count:55 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |