Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 80.4 MPa | 11700 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN131 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Tensile Strength, Ultimate | 80.4 MPa | 11700 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN3322VO Flame Retardant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Tensile Strength, Ultimate | 80.4 MPa | 11700 psi | DIN 53455; ASTM D638 |
Kolon NOPLA® KE911 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Tensile Strength, Ultimate | 81.0 MPa @Temperature 22.0 °C |
11700 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Tensile Strength, Ultimate | 80.4 MPa | 11700 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN133HR Heat Resistant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Tensile Strength, Ultimate | 80.4 MPa | 11700 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN171 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Tensile Strength, Ultimate | 81.0 MPa | 11700 psi | ISO 527-1, 2 |
Polyplastics Duranex® 3100H Polybutylene Terephthalate (PBT), Standard, 7.5% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Tensile Strength, Ultimate | 81.0 MPa | 11700 psi | ATSM D638 |
Ashley Polymers Ashlene® 528L Nylon 66 General purpose injection molding grade.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 81.0 MPa | 11700 psi | ATSM D638 |
Ashley Polymers Ashlene® 528LW Nylon 66 General purpose injection molding grade.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 81.0 MPa | 11700 psi | ATSM D638 |
Ashley Polymers Ashlene® 539L Nylon 66 High viscosity for injection molding of heavy parts.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 81.0 MPa @Temperature 982 °C |
11700 psi @Temperature 1800 °F |
ASTM E8 |
ATI Allegheny Ludlum 310S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 81.0 MPa | 11700 psi | ASTM D638 |
A. Schulman ComAlloy Aqualoy® 135 Polypropylene, Glass Reinforced, Chemically Coupled NSF, UL Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Tensile Strength, Ultimate | 81.0 MPa | 11700 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 124 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 81.0 MPa | 11700 psi | ATSM D638 |
Ashley Polymers Ashlene® 539 Nylon 66 Extrusion grade for film & monofilament.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 81.0 MPa | 11700 psi | ASTM D638 |
A. Schulman ComAlloy Aqualoy® 134 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Tensile Strength, Ultimate | 81.0 MPa | 11700 psi | ASTM D638 |
A. Schulman ComAlloy Aqualoy® 145 Polypropylene, Glass Reinforced, Chemically Coupled NSF Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Tensile Strength, Ultimate | 81.0 MPa | 11700 psi | ASTM D638 |
A. Schulman ComAlloy Lubrilon® 631 Nylon 6/6, Graphite/Molybdenum Disulfide Filled Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Tensile Strength, Ultimate | 81.0 MPa | 11700 psi | DIN 53455; ASTM D638 |
Kolon Kopa® KN153G15 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |