Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 8.10 MPa | 1170 psi | |
Kuraray SEPTON® H5125 Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Strength, Ultimate | 8.07 MPa | 1170 psi | no post cure; ASTM D412 |
Multibase C6-515 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Ultimate | 8.07 MPa | 1170 psi | ASTM D638 |
Multibase Multi-Flamâ„¢ 0803 LDPE NH Yellow Polyethylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Ultimate | 8.07 MPa | 1170 psi | |
Dow Corning C6-165 ELASTOMER KIT Two-part, platinum-catalyzed (1:1 by weight), silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices, and fabricating extruded.. |
|||
Tensile Strength, Ultimate | 8.10 MPa | 1170 psi | GB/T 528 |
Chengdu Polyster 7502 High Performance Grade TPV Excellent resiliency, good hand feel, paintable.Information provided by Chengdu Polyster Co., Ltd. |
|||
Tensile Strength, Ultimate | 8.07 MPa | 1170 psi | |
Dow Corning SILASTIC® 25140 SILICONE RUBBER 40 durometer, peroxide cured, general purpose silicone rubber compoundInformation provided by Dow Corning |
|||
Tensile Strength, Ultimate | 8.07 MPa | 1170 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2060 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |