Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 11.3 MPa | 1640 psi | |
Colorite Polymers Flexchem 5551-02 Vinyl Compound Description: The Flexchem "51" series is a group of translucent, flexible, non-toxic vinyl compounds which were specifically developed to replace silicone in various applications. These compounds ut.. |
|||
Tensile Strength, Ultimate | 11.3 MPa | 1640 psi | ASTM D638 |
Colorite Polymers MULTICHEM™ 6014 Vinyl-Urethane Blend Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers. |
|||
Tensile Strength, Ultimate | 11.3 MPa | 1640 psi | ASTM D638 |
Colorite Polymers 6014 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 11.3 MPa | 1640 psi | Across Flow; ASTM D412 |
ExxonMobil Geolast® 703-45 Thermoplastic Elastomer A hard, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |