Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 105.9 MPa | 15360 psi | ASTM D638 |
Plenco 51240 PET, Pellet, Injection Molded, Blue
(discontinued **) PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P.. |
|||
Tensile Strength, Ultimate | 105.9 MPa @Temperature 150 °C |
15360 psi @Temperature 302 °F |
ASTM D638 |
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |