Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 6.950 MPa | 1008 psi | |
Dow Corning SILASTIC® 25785-V SILICONE RUBBER RED 50 Durometer, peroxide cured, high temperature resistance Silicone Rubber CompoundInformation provided by Dow Corning |