Polymer Property : Tensile Strength, Ultimate = 10.63 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.63 MPa
1542 psi
as molded
Multibase SILASTIC® C7-4550 DICUP R Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase