Polymer Property : Tensile Strength, Ultimate = 0.800 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.800 - 80.0 MPa
116 - 11600 psi
Average value: 29.0 MPa Grade Count:318
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..
Tensile Strength, Ultimate 0.800 - 68.9 MPa
116 - 10000 psi
Average value: 26.1 MPa Grade Count:120
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..
Tensile Strength, Ultimate 0.800 MPa
116 psi
ASTM D 638
REXtac Rextac® RT 2385 Amorphous Polyalphaolefin (APAO)
Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance of heat resistance, flexibility, stiffness, high viscosity, and medium open timeApplications: Component ..